Properti | Metode Tes | Nilai standar |
Suhu Operasi | IEC 216 | -45 ℃ kanggo 105 ℃ |
Kekuwatan Tensile | ASTM-D-2671 | ≥12MPa |
Elongation ing Break | ASTM-D-2671 | ≥300% |
Kekuwatan Tensile Sawise Aging | ASTM-D-2671 | ≥10MPa (130 ℃, 168 jam) |
Elongation ing Break | ASTM-D-2671 | ≥230% (130 ℃, 168 jam) |
sawise Aging | ||
Kekuwatan dielektrik | IEC 60243 | ≥20kV/mm |
Stress Cracking Resistance | ASTM-D-1693 | Ora retak |
Resistivitas Volume | IEC 60093 | ≥1×1014Ω·cm |
Ketahanan jamur lan bosok | ISO 846 | Lulus |
Penyusutan longitudinal | ASTM-D-2671 | ≤10% |
Eksentrisitas | ASTM-D-2671 | ≤30% |
Penyerapan banyu | ISO 62 | ≤0,5% |
Ukuran | D/mm | L/mm | W/mm | ||
Minangka diwenehake | Sawise pulih | ||||
Minangka diwenehake | Sawise pulih | ||||
11/6 | ≥11 | ≤6 | ≥22 | 0,7 ± 0,1 | ≤1.1 |
16/8 | ≥16 | ≤8 | ≥70 | 1.2±0.1 | ≤2.2 |
20/8 | ≥20 | ≤8 | ≥70 | 1.2±0.1 | ≤2.2 |
25/11 | ≥25 | ≤11 | ≥80 | 1.2±0.1 | ≤2.3 |
32/16 | ≥32 | ≤16 | ≥90 |